To avoid stress corrosion cracking, the filler alloy used for elevated temp application is AA-5554, which has 3% max Mg.

Study for the Canadian Welding Bureau (CWB) Level 3 Exam. Practice with flashcards and multiple choice questions, each question is accompanied by helpful hints and explanations. Prepare thoroughly and boost your exam confidence!

Multiple Choice

To avoid stress corrosion cracking, the filler alloy used for elevated temp application is AA-5554, which has 3% max Mg.